Pure Lead Ingots are produced from Raw Lead Bullions/ Remelted Lead Ingots/ Secondary Lead Ingots / Lead Scraps through Pyro Metallurgical process. Our refining process produces Pure Lead Ingots with a purity level of 99.97% to 99.985% by weight.
Our Plant is having four Refining Kettles with capacity of 30 MT, 16 MT, 10 MT and 7 MT. Automatic Ingot Casting Machine casts 10 MT ingots per hour and ensures Dross-Free, smooth top surface and uniform weight of each ingot.
The typical composition of Refined Lead /
Pure Lead -

|
Elements |
Symbol |
Composition in % |
|
Antimony |
Sb |
0.001 (max) |
|
Arsenic |
As |
0.001 (max) |
|
Tin |
Sn |
0.001 (max) |
|
Copper |
Cu |
0.001 (max) |
|
Bismuth |
Bi |
0.015 (max) |
|
Iron |
Fe |
0.001 (max) |
|
Nickel |
Ni |
0.001 (max) |
|
Silver |
Ag |
0.003 (max) |
|
Zinc |
Zn |
0.001 (max) |
|
Calcium |
Ca |
0.0005 (max) |
|
Sulphur |
S |
0.0005 (max) |
|
Aluminum |
Al |
0.0005 (max) |
|
Selenium |
Se |
0.0005 (max) |
|
Cadmium |
Cd |
0.0005 (max) |
|
Tellurium |
Te |
0.0010 (max) |
|
Lead |
Pb |
99.970 (min) |